The document reports on a biodegradation test of perfluorooctanesulfonylamido(ethyl)acetate (PFOSAA or FC-128), indicating that approximately 70% of the theoretical maximum oxygen uptake occurred within a 7-hour period, suggesting potential biodegradability under the tested conditions.
|